Selasa, 21 Juli 2009

STANDAR MATERIAL

STANDAR MATERIAL

1. C75.75 For main Structure

A. Hi-tensile Zincalume – Grade 550 (5500 Kg/cm2)

b. Properties :

D (Depth)

75.00 mm

T (thickness)

0.75 mm

Mass per unith Length

1.31 Kg/m

Ix

0.105 x10^6 mm^4

Zx

2.68 x 10^3 mm^3

Zy

0.74 x 10^ mm^3

Y (min yield stress)

550.00 Mpa

Py(design strength)

550.00 Mpa

2. C75.100 For main Structure

A. Hi-tensile Zincalume – Grade 550 (5500 Kg/cm2)

b. Properties :

D (Depth)

75.00 mm

T (thickness)

1.00 mm

Mass per unith Length

1.55 Kg/m

Ix

0.140 x10^6 mm^4

Zx

3.64 x 10^3 mm^3

Zy

1.01 x 10^ mm^3

Y (min yield stress)

550.00 Mpa

Py(design strength)

550.00 Mpa

3 C100.100 For main Structure

A. Hi-tensile Zincalume – Grade 550 (5500 Kg/cm2)

b. Properties :

D (Depth)

100.00 mm

T (thickness)

1.00 mm

Mass per unith Length

1.88 Kg/m

Ix

0.347 x10^6 mm^4

Zx

6.54 x 10^3 mm^3

Zy

2.04 x 10^ mm^3

Y (min yield stress)

550.00 Mpa

Py(design strength)

550.00 Mpa

4. TS 40.048 for Batten

A. Hi-tensile Zincalume – Grade 550 (5500 Kg/cm2)

b. Properties :

D (Depth)

40.00 mm

T (thickness)

0.48 mm

Mass per unith Length

1.55 Kg/m

Ix

0.140 x10^6 mm^4

Zx

3.64 x 10^3 mm^3

Zy

1.01 x 10^ mm^3

Y (min yield stress)

550.00 Mpa

Py(design strength)

550.00 Mpa